dc.description.abstract A study was conducted on four commercial Waxy Oil green cokes with varying catalyst (Fe3O4) concentrations (ash content: 1.84–11.18%), to determine the effect thereof on the structural characteristics of calcined (1400 C) and pre-graphitised (2000 C) cokes. An increase in the catalyst content of the coke shows a substantial detrimental effect on the overall anisotropy of the carbon microtexture. Catalyst particles below 100 lm) were found to present a physical barrier around which the anisotropic flow domains formed. At higher catalyst concentrations the catalyst dominates the carbon microtexture; however, there is still evidence of flow patterns albeit with a shorter range. XRD powder data and Raman spectroscopy provide evidence of multiphase graphitisation in both the calcined coke and pre-graphite. The crystal development of the calcined coke is dominated by catalytic graphitisation and that of the pregraphite showed a greater dependence on thermal graphitisation. This is the first scientific study of the effect of catalyst concentration on the characteristics of this novel coke and proves the disingenuous comparability thereof with a highly anisotropic coke (e.g. needle coke). en_US
dc.description.uri http://www.elsevier.com/locate/fuel en_US
dc.identifier.citation Clark, JG, Rand, B, Hayes, MP, Barnard, W & Lubhelwana, S, The effect of an iron oxide catalyst (Fe3O4) on the characteristics of Waxy Oil coke, Fuel, vol. 94, pp. 523–531 (2012), doi:10.1016/j.fuel.2011.09.051. en_US
dc.identifier.issn 0016-2361 (print)
dc.identifier.issn 1873-7153 (online)
dc.identifier.other 10.1016/j.fuel.2011.09.051
dc.identifier.uri http://hdl.handle.net/2263/18405
dc.language.iso en en_US
dc.publisher Elsevier en_US
dc.rights © 2011 Elsevier Ltd. All rights reserved. Notice : this is the author’s version of a work that was accepted for publication in Fuel. Changes resulting from the publishing process, such as peer review, editing, corrections, structural formatting, and other quality control mechanisms may not be reflected in this document. Changes may have been made to this work since it was submitted for publication. A definitive version was subsequently published in Fuel, vol. 94, pp. 523–531 (2012), doi:10.1016/j.fuel.2011.09.051. en_US
dc.subject Waxy Oil coke en_US
dc.subject Catalyst en_US
dc.subject Reactivity en_US
dc.subject Multiphase graphitisation en_US
dc.subject Microstructure en_US
dc.title The effect of an iron oxide catalyst (Fe3O4) on the characteristics of Waxy Oil coke en_US
dc.type Postprint Article en_US


Files in this item

This item appears in the following Collection(s)

Show simple item record