The effect of scan speed and hatch distance on prior-beta grain size in laser powder bed fused Ti-6Al-4V

Loading...
Thumbnail Image

Authors

Louw, D.F.
Pistorius, Pieter Georg Hendrik

Journal Title

Journal ISSN

Volume Title

Publisher

Springer

Abstract

Ti-6Al-4V produced by laser powder bed fusion can achieve mechanical properties similar to its wrought counterpart if an appropriate post-process heat treatment is applied. The response of the material to post-process heat treatment depends on the prior-beta grain size in the as-built condition. The current article illustrates that a reduction in hatch distance can cause coarsening of prior-beta grains due to retained heat that reduces the cooling rate. On the other hand, an increase in scan speed refines prior-beta grains. Unfortunately, an increase in scan speed has to be accompanied by a reduction in hatch distance to prevent an increase in porosity and the potential grain refinement is then cancelled out. The use of a faster scan speed in combination with a smaller hatch distance significantly improves roughness of the top surface. EBSD in combination with reconstruction of prior-beta grains is an effective technique to quantify prior-beta grain size. Furthermore, the use of Rosenthal’s equations allows quick calculation of cooling rate that can be used to predict the dependence of prior-beta grain size on process parameters.

Description

Keywords

Titanium metallurgy, Selective laser melting, Additive manufacturing, Laser powder bed fusion (LPBF)

Sustainable Development Goals

Citation

Louw, D.F. & Pistorius, P.G.H. The effect of scan speed and hatch distance on prior-beta grain size in laser powder bed fused Ti-6Al-4V. International Journal of Advanced Manufacturing Technology (2019) 103: 2277-2286 https://doi.org/10.1007/s00170-019-03719-w.