Kambilinya, Patrick Isaac Edwin
(University of Pretoria, 2021)
The requirement for a combination of high yield strength (≥345 MPa)and impact toughness at low temperatures, typically, CVN 40 to 60 J at –20 °C, is stringent in wind tower applications of normalised Nb-Ti-V and VN ...